4.7 Article

3D anisotropic conductive fibers electrically stimulated myogenesis

期刊

出版社

ELSEVIER
DOI: 10.1016/j.ijpharm.2021.120841

关键词

Nanofibers; Tissue engineering; Myogensis; Electrical stimulation; Melt electrowriting

资金

  1. Carlsberg Foundation [CF19-0300]
  2. Aarhus University Research foundation [AUFF-E-2015-FLS-7-27]
  3. China Scholarship Council

向作者/读者索取更多资源

The study demonstrates the effectiveness of using anisotropic scaffolds along with electrical stimulation to promote elongation and maturation of muscle cells. The alignment and elongation of myotubes were significantly enhanced under electrical stimulation on the anisotropic scaffold, providing a promising platform for skeletal muscle tissue engineering.
Recapitulation of in vivo environments that drive muscle cells to organize into a physiologically relevant 3D architecture remains a major challenge for muscle tissue engineering. To recreate electrophysiology of muscle tissues, electroactive biomaterials have been used to stimulate muscle cells with exogenous electrical fields. In particular, the use of electroactive biomaterials with an anisotropic micro-/nanostructure that closely mimic the native skeletal-muscle extracellular matrix (ECM) is desirable for skeletal muscle tissue engineering. Herein, we present a hierarchically organized, anisotropic, and conductive Polycaprolactone/gold (PCL/Au) scaffold for guiding myoblasts alignment and promoting the elongation and maturation of myotubes under electrical stim-ulation. Culturing with H9c2 myoblasts cells indicated that the nanotopographic cues was crucial for nuclei alignment, while the presence of microscale grooves effectively enhanced both the formation and elongation of myotubes. The anisotropic structure also leads to anisotropic conductivity. Under electrical stimulation, the elongation and maturation of myotubes were significantly enhanced along the anisotropic scaffold. Specifically, compared to the unstimulated group (0 V), the myotube area percentage increased by 1.4, 1.9 and 2.4 times in the 1 V, 2 V, 3 V groups, respectively. In addition, the myotube average length in the 1 V group increased by 1.3 times compared to that of the unstimulated group, and significantly increased by 1.8 and 2.0 times in the 2 V, 3 V groups, respectively. Impressively, the longest myotubes reached more than 4 mm in both 2 V and 3 V groups. Overall, our conductive, anisotropic 3D nano/microfibrous scaffolds with the application of electrical stimulation provides a desirable platform for skeletal muscle tissue engineering.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据