4.6 Article

Comprehensive Annealing Effects on AlGaN/GaN Schottky Barrier Diodes With Different Work-Function Metals

期刊

IEEE TRANSACTIONS ON ELECTRON DEVICES
卷 68, 期 6, 页码 2661-2666

出版社

IEEE-INST ELECTRICAL ELECTRONICS ENGINEERS INC
DOI: 10.1109/TED.2021.3074896

关键词

Lateral GaN Schottky barrier diode (SBD); postanode-annealing; various work-function metals

资金

  1. National Key Research and Development Program [2018YFB0406601, 2016YFB0400100]
  2. National Natural Science Foundation of China [62004152]

向作者/读者索取更多资源

This article systematically investigates the impact of annealing on GaN SBDs and the anode metals on the performance of AlGaN/GaN SBDs. It was found that annealing treatment can suppress interface states, enhance device stability, and achieve high-performance SBDs with various work-function metals as anodes. Different Schottky barrier heights and characteristics were obtained with different metals, with W providing a low turn-on voltage and low leakage current, and Ni showing extremely low leakage current and great characteristics at high temperature.
In this article, we have systematically investigated the effect of annealing of fabricated GaN Schottky barrier diodes (SBDs) and anode metals with various work-functions on the performance of AlGaN/GaN SBDs. It is found that after annealing of fabricated GaN SBDs, the interface states between the metal and GaN etching surface are suppressed, the device stability is enhanced, and the turn-on voltage (V-ON) shows negligible degradation. Meanwhile, high-performance AlGaN/GaN SBDs with various work-function metals as anode have been achieved by adapting the annealing treatment. The calculated Schottky barrier heights of the fabricated SBDs with Cr, W, and Ni anode is 0.27, 0.68, and 0.98 eV, respectively, which are almost the same as those estimated from XPS measurements. A low turn-on voltage of 0.42 V and low leakage current of 0.3 mu A/mm are obtained by using the low work-function metal W (4.6 eV) as anode. Furthermore, the SBDs fabricated with the high work-function metal Ni (5.1 eV) shows an extremely low-leakage current of 6 nA/mm and exhibit a current ON/OFF ratio of 10(9) while also showing great characteristics at high temperature.