PECULIARITIES OF SOL-GEL SYNTHESIS OF ALUMINUM-MAGNESIUM SPINEL

期刊

GLASS AND CERAMICS
卷 78, 期 5-6, 页码 251-254

出版社

SPRINGER
DOI: 10.1007/s10717-021-00389-7

关键词

aluminum-magnesium spinel; sol-gel method; alumina-containing waste; phase transformations; x-ray phase analysis; gamma-aluminum oxide-aluminum

向作者/读者索取更多资源

The optimal conditions for synthesizing MgAl2O4 spinel using alumina-containing waste in the gas processing industry were found to be soaking at a temperature of 1000 degrees Celsius for 120 minutes.
The results of studies of the chemical and mineralogical characteristics of alumina-containing wastes of the gas processing industry and the possibilities of their use for the synthesis of aluminum-magnesium spinel are presented. The optimal condition for the synthesis of MgAl2O4 spinel by the sol-gel method using alumina-containing waste is found to be 1000 degrees C temperature and 120 min soaking.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.1
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据