Achieving adequate manganese removal during water treatment is challenging. Gravity-driven ceramic membrane filtration was effective in eliminating manganese from surface water. Pre-coating membranes with manganese oxides and reducing molecular weight cut-off improved long-term treatment efficiency, with 15 kDa membrane achieving the highest removal efficiency of 75%.
Achieving adequate manganese removal during water treatment is a challenging process. This study aimed to assess the effectiveness of gravity driven ceramic membrane (GDCM) filtration in the elimination of manganese from surface water. The impact of membrane pre-modification with birnessite and molecular weight cut-off on long-term water treatment efficiency was investigated by assessing filtration units with 300 kDa virgin membrane (300 kDa-blank), 300 kDa membrane pre-coated with manganese oxides (300 kDa-MnOx), and 15 kDa virgin membrane (15 kDa-blank). The results of 300 kDa-blank and 300 kDa-MnOx indicated that depositing manganese oxides (produced via ozone (O-3) oxidation) prior to water treatment was conducive to ripening of cake layer which played a major role in Mn removal. Reducing membrane molecular cut-off from 300 to 15 kDa also significantly reduced permeate Mn concentration, achieving a removal efficiency of 75% at the end of the trial (highest of all the units). Relative to 300 kDa-blank, the greater manganese removals in the other two systems can be attributed to 1) the long hydraulic retention times resulting from the higher membrane resistance, and 2) the higher abundance of biologically produced Birnessite materials in the cake layers for manganese oxidation. Raman analysis and X-ray diffraction analysis showed that 15 kDa-blank achieved the highest level of Birnessite production and most cake materials featured a flower-like structure and relatively small size (as shown under a scanning electron microscope and Energy Dispersive X-Ray Spectroscopy element mapping analysis), suggesting a higher surface area for Mn oxidation. (C) 2021 Elsevier Ltd. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据