Fracture resistance of AlSi10Mg fabricate d by laser powder b e d fusion

期刊

ACTA MATERIALIA
卷 211, 期 -, 页码 -

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.actamat.2021.116869

关键词

AlSi10Mg; Laser powder bed fusion; Microstructure and mesostructure; Crack resistance curve ( R-curve) behavior; Mechanical properties

资金

  1. UNSW Scientia Fellowship
  2. Australian Research Council (ARC) Discovery Early Career Researcher Award (DECRA) [DE190101495]
  3. A STAR, Singapore via the Structural Metals and Alloys Programme [A18B1b0061]
  4. Australian Research Council [DE190101495] Funding Source: Australian Research Council

向作者/读者索取更多资源

The combination of refined microstructures induced by rapid cooling and melt pool-induced mesostructures in LPBF-fabricated AlSi10Mg plays a crucial role in imparting high strength and fracture toughness. Understanding the relationship between processing conditions, micro-and mesostructures, and mechanical performance is key to further exploiting these property combinations.
The combination of refined microstructures (induced by rapid cooling) and melt pool-induced mesostructures in AlSi10Mg fabricated using laser powder bed fusion (LPBF) - a widely used additive manufacturing technique -impart high strength and fracture toughness. Further exploitation of such property combinations requires a detailed understanding of how the processing conditions control the micro-and mesostructures and, in turn, the mechanical performance, especially regarding fracture resistance. Towards this end, the crack resistance curve ( R-curve) behavior in different orientations of LPBF-fabricated AlSi10Mg alloys processed with different layer thickness, hatch spacing, and scan strategies was evaluated and correlated with micro-and mesostructural features such as grain size and grain orientation, texture, cell morphology, and melt pool arrangement. Results show a strong anisotropy in both tensile stress strain behavior and fracture toughness with layer thickness and hatch spacing controlling strength and scan strategy dictating fracture resistance. In terms of tensile stress-strain behavior, the arrangement of melt pool boundaries with respect to loading direction results in anisotropy in ductility whereas strength is controlled by grain size and cellular structure. In case of fracture toughness, measurements show that failure is dominated primarily by melt pool morphology and hence the mesostructure that is controlled by scan strategy. They furthermore reveal, that, despite the pronounced anisotropy in the R-curve behavior the presence of such mesostructure enables a level of damage-tolerance in AlSi10Mg that cannot be achieved in a cast alloy. (c) 2021 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据