Effect of biodegradation on thermo-mechanical properties and biocompatibility of poly(lactic acid)/graphene nanoplatelets composites

期刊

EUROPEAN POLYMER JOURNAL
卷 85, 期 -, 页码 431-444

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.eurpolymj.2016.10.046

关键词

Creep-recovery; Tensile tests; X-ray diffraction; Gel permeation chromatography and size; exclusion chromatography (GPC-SEC); Biodegradation assays

资金

  1. Fundacao para a Ciencia e a Tecnologia (FCT) [SFRH/BD/86974/2012]
  2. European Social Fund
  3. Portuguese Ministry of Education and Science (MEC) through Programa Operacional Capital Humano (POCH)
  4. Laboratory for Process Engineering, Environment, Biotechnology and Energy - LEPABE [POCI-01-0145-FEDER-006939]
  5. Institute for Research and Innovation in Health Sciences - FEDER funds through COMPETE - Programa Operacional Competitividade e Internacionalizacao (POCI) - and by national funds through FCT - Fundacao para a Ciencia e a Tecnologia [POCI-01-0145-FEDER-007274]
  6. Fundação para a Ciência e a Tecnologia [SFRH/BD/86974/2012] Funding Source: FCT

向作者/读者索取更多资源

Two types of graphene nanoplatelets (GNP-M and GNP-C) were incorporated in PLA by melt-blending at 0.25 wt.% loading, and the resulting composites subject to hydrolytic degradation for 6 months in phosphate-buffered saline (PBS) at 37 C. The materials were characterized by Fourier transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), size exclusion chromatography (GPC-SEC), scanning electron microscopy (SEM), thermogravimetric analysis (TGA), differential scanning calorimetry (DSC), tensile testing, creep recovery testing, and biocompatibility assays. After two months degradation, all materials presented a low decrease in molecular weight (about 10%), while after six months the decrease was higher than 85%. For this degradation time, temperatures of onset of intense thermal degradation decreased by about 10 C for all samples. Both fillers were able to improve the mechanical properties of PLA, and to reduce the decay of its mechanical performance after 6 months biodegradation. Unfilled PLA showed a 10-fold decrease in toughness (AUC) after 6 months degradation, while toughness was only reduced by 3.3 and 1.7-fold, respectively, for the GNP-M and GNP-C composites. In addition, the composites had stable behaviour under cyclic creep-relaxation testing, while PLA exhibited significant cumulative permanent stain and ruptured after only 4 cycles. Comparing with PLA, the GNP-based composites presented similar human foreskin fibroblasts (HFF-1) adhesion and growth at the surface until 72 h, and did not release toxic products after the degradation period. (C) 2016 Elsevier Ltd. All rights reserved.