Experimental Study of Tensile Properties of Styrene-Butadiene-Styrene Modified Asphalt Binders

期刊

MATERIALS
卷 14, 期 7, 页码 -

出版社

MDPI
DOI: 10.3390/ma14071734

关键词

asphalt binder; styrene– butadiene– styrene copolymer; force ductility test; rheology; modified bitumen

向作者/读者索取更多资源

This article presents the results of tests conducted on bitumens modified with two types of styrene-butadiene-styrene copolymer (linear and radial). It was found that the effectiveness of the modification varied with the type of copolymer added.
The requirements imposed on road pavements are ever increasing nowadays, necessitating the improvement of the properties of paving materials. The most commonly used paving materials include bituminous mixtures that are composed of aggregate grains bound by a bituminous binder. The properties of bitumens can be improved by modification with polymers. Among the copolymers used for modifying bitumens, styrene-butadiene-styrene, a thermoplastic elastomer, is the most commonly used. This article presents the results of tests conducted on bitumens modified with two types of styrene-butadiene-styrene copolymer (linear and radial). Two bitumen types of different penetration grades (35/50 and 160/220) were used in the experiments. The content of styrene-butadiene-styrene added to the bitumen varied between 1% and 6%. The results of the force ductility test showed that cohesion energy can be used for qualitative evaluation of the efficiency of modification of bitumen with styrene-butadiene-styrene copolymer. The determined values of the cohesion energy were subjected to the original analysis taking into account the three characteristic elongation zones of the tested binders. The performed analyses made it possible to find a parameter whose values correlate significantly with the content of styrene-butadiene-styrene copolymer in the modified bitumen. With smaller amounts of added modifier (approximately 2%), slightly better effects were obtained in the case of linear copolymer styrene-butadiene-styrene and for larger amounts of modifier (5-6%) radial copolymer styrene-butadiene-styrene was found to be more effective. This is confirmed by the changes in the binder structure, as indicated by the penetration index (PI).

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据