4.7 Article

Evaluating the total gold concentration in metallic nanoparticles with a high content of organic matter through microwave-assisted decomposition platform and plasma-based spectrometric techniques (ICP-MS and ICP OES)

期刊

TALANTA
卷 224, 期 -, 页码 -

出版社

ELSEVIER
DOI: 10.1016/j.talanta.2020.121808

关键词

Elemental analysis; Gold concentration; Metallic nanoparticles; Microwave-assisted decomposition; Sample preparation

资金

  1. Coordenacao de Aperfeicoamento de Pessoal de Nivel Superior (CAPES) - Brazil [001]
  2. Fundacao de Amparo a Pesquisa do Estado de Sao Paulo (FAPESP) - Brazil [2018/252070, 2019/24445-8]
  3. Conselho Nacional de Desenvolvimento Cientifico e Tecnologico (CNPq) - Brazil

向作者/读者索取更多资源

A complete set of strategies for accurate determination of gold in metallic nanoparticles has been reported. By overcoming the challenges posed by the surfactant CTAB, a microwave-assisted decomposition platform demonstrated to be an efficient and reliable tool for gold quantification in metallic nanoparticles. The proposed strategies provide an accurate recovery of gold content with no interference of the complex matrix.
We report a complete set of strategies for characterization and an accurate determination of gold in metallic nanoparticles. For this, gold nanorods (AuNR) were synthesized by using the surfactant hexadecyltrimethylammonium bromide (CTAB) as the stabilizer and shape-directing agent. The surfactant CTAB forms a bilayer structure around the nanoparticles and became a challenge for the development of the microwaveassisted decomposition of the AuNR colloid. The bilayer structure of CTAB prevents the Au3+ release for the acidic media during the decomposition procedure. To overcome this limitation, a combination of low sample volume consumption (only 200 mu L), an acidic mixture of reverse aqua regia (1:3 v/v, HCl:HNO3), and sulfuric acid, and a microwave program was used. The gold quantification by ICP-MS and checked through the ICP OES, demonstrated that the seed-mediated growth method used for the AuNR synthesis has a high yield, presenting ca. 100% of gold content (ca. 100 mg L-1 of gold concentration) in the post-synthesis colloid (AuNR-total) as well as in the colloid after a washing step (AuNR-res). The microwave-assisted decomposition procedure also demonstrated to be efficient in the acidic decomposition of the gold-silver core-shell nanoparticle (Au@AgNR), which presents a high content of polyvinylpyrrolidone (PVP) (Mw similar to 55000 g mol(-1)) acting as a stabilizer, in addition to the matrix with CTAB. The results demonstrated an accurate recovery of ca. 100% of gold content for the Au@AgNR regarding the gold nanorod before the growth of the silver shell (AuNR_Core). The proposed microwave-assisted decomposition platform demonstrated to be an efficient, reliable, and robust characterization tool for the gold quantification in metallic nanoparticles, presenting no interference of the complex matrix with high organic content.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据