Preparation of Li7P3S11 glass-ceramic electrolyte by dissolution-evaporation method for all-solid-state lithium ion batteries

期刊

ELECTROCHIMICA ACTA
卷 219, 期 -, 页码 235-240

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.electacta.2016.09.155

关键词

Li7P3S11 glass-ceramic; Solid state electrolyte; Lithium ion battery; Ion conductivity

资金

  1. program for Innovative Research Team in University of Ministry of Education of China [IRT13037]

向作者/读者索取更多资源

Design/fabrication of solid state electrolytes with high ionic conductivity is of great importance to develop next-generation Li ion batteries. In this work, the Li7P3S11 glass-ceramic electrolyte is successfully synthesized by dissolution-evaporation approach. The solvent effect on the electrochemical performance of Li7P3S11 is investigated by electrochemical impedance spectroscopy and chronoamperometry tests. The Li7P3S11 electrolyte prepared by a solution of acetonitrile has a high ionic conductivity of 9.7 x 10(-4) S cm(-1) at 298 K and a low activation energy of 31.2 kJ mol-(1). Impressively, a wide and stable electrochemical window up to 5 V (vs. Li/Li+) is demonstrated between the solid electrolyte and lithium electrode. The developed dissolution-evaporation approach shows good industrial prospect due to its advantages of energy conservation and high efficiency. (C) 2016 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据