4.7 Article

Corrosion behavior of cold sprayed 7075Al composite coating reinforced with TiB2 nanoparticles

期刊

SURFACE & COATINGS TECHNOLOGY
卷 404, 期 -, 页码 -

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/j.surfcoat.2020.126460

关键词

Particle reinforced Al matrix composites; Cold spraying; TiB2 reinforcement; Aqueous corrosion

资金

  1. China Scholarship Council
  2. Campus France through the PHC Xu Guangqi program [45597XK]

向作者/读者索取更多资源

Cold spray (CS), as a novel surface treatment technique, has been widely used for repairing damaged components and as protecting coatings, especially for the applications of aircraft and marine components. To further improve the mechanical properties, while maintaining the corrosion resistance of pure Al and Al alloy coatings, ceramic particles are commonly added into the Al matrix to produce particle-strengthened Al matrix composite (P-AMC) coatings. In this study, dense 7075Al composite coatings reinforced with uniformly distributed in-situ TiB2 nanoparticles (hereafter named TiB2/7075Al) were successfully produced by CS using a gas-atomized composite powder and the propulsive gases of air and helium. Following this, the corrosion behavior of the cold sprayed (CSed) TiB2/7075Al composites was investigated using Tafel polarization, electrochemical impedance, spectroscopy, and immersion tests in 0.1 M and 0.6 M NaCl solutions, and were compared to those of the CSed pure 7075Al coating and bulk 7075Al-T6 material. Electrochemical tests revealed that the composite coating exhibits a higher corrosion rate than the pure 7075Al coating, primarily caused by a galvanic coupling between TiB2 nanoparticles and the more active Al matrix. Compared to the air-processed coatings, the He-processed ones exhibit higher densities of defects, like dislocations, and precipitates due to larger plastic deformation of the sprayed particles, which result in more active sites for corrosion and thus lower corrosion resistance. Low-temperature annealing treatment (230 degrees C/6 h) reduces these defects to increase the corrosion resistance of the CSed coatings. Comparatively, high-temperature annealing treatment (412 degrees C/4 h) results in the coarsening of precipitates and grain growth to increase the corrosion rate of the coatings. Corrosion mechanisms of the CSed and annealed composite coatings related to the microstructure evolution were investigated in detail.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据