4.6 Article

Device performance of chemical vapor deposition monocrystal diamond radiation detectors correlated with the bulk diamond properties

期刊

出版社

IOP PUBLISHING LTD
DOI: 10.1088/1361-6463/abd5e2

关键词

Type IIa CVD diamond; radiation detectors; charge collection efficiency; material defects

资金

  1. National Natural Science Foundation of China [61874080, 62004148]
  2. National Key Research and Development Program of China [2018YFB0406504]
  3. Natural Science Basic Research Program of Shaanxi [2020JQ-315]
  4. China Postdoctoral Science Foundation [2019M663627]
  5. Fundamental Research Funds for the Central Universities [XJS201101]
  6. Natural Science Basic Research Plan in Shaanxi Province of China program [2019ZDLGY16-02]
  7. Open Fund of Key Laboratory of High Power Microwave [6142605180102, 6142605190203]

向作者/读者索取更多资源

The study found that impurities in diamond plates have the most significant impact on the performance of diamond radiation detectors, while dislocations have a weaker effect on CCEs. Moreover, maintaining a thickness of diamond plates above 100μm is crucial for obtaining high-performance detectors.
Diamond radiation detectors (DRDs) based on type-IIa chemical vapor deposition (CVD) monocrystal diamond are more suitable for engineering applications with high consistency requirements due to the lower cost and property controllability. However, their saturated charge collection efficiencies (CCEs) have huge differences. Six type-IIa CVD monocrystal diamond plates were analyzed by the Fourier transform infrared spectrometer, high resolution x-ray diffraction, Raman spectroscopy, photoluminescence and secondary ion mass spectroscopy. Then DRDs were fabricated by them and the CCEs were measured under the irradiation of Am-241 source. The results show that the most important factor restricting CCEs are the impurities in the diamond plates, while dislocations with a density <1 x 10(7) cm(-2) for all samples have weaker impact in our case. The reason is that the carrier mobility-lifetime (mu tau) product of diamond is more strongly influenced by impurities in this dislocation density range. Thinning diamond plate, if the thickness is kept above 100 mu m, is not a good means to obtain high performance DRDs. Therefore, to further improve the detector performance, ultra-high purity diamond growth is most important. Moreover, a diamond test and selection scheme for high performance DRDs is also demonstrated.