Fine-grain heat affected zone softening of G115/Sanicro25 dissimilar steel welded joints after post-weld heat treatment

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.ijpvp.2020.104253

关键词

Dissimilar steel welded joint; Fine grain heat affected zone(FGHAZ); Dislocation density; Martensite lath; Strengthening mechanism

资金

  1. National Key R&D Program of China [2016YFC0801902]
  2. Shenhua Guohua (Beijing) Electric Power Research Institute Co., Ltd.

向作者/读者索取更多资源

The mechanical properties of the G115/Sanicro25 dissimilar steel welded joints were characterized by room temperature tensile and microhardness. The microstructures of fine-grain heat affected zone (FGHAZ) and base metal (BM) in the G115 steel side were characterized by optical microscopy, SEM, TEM, and XRD. The results show that as the strain increases, weld beam first yields and hardens, the stress on the specimen is further increased, then Sanicro25 steel yields and hardens, and G115 steel yields finally, the specimen broken in the FGHAZ of G115 steel side. The FGHAZ of G115 steel side softens after post-weld heat treatment (PWHT). The size of the heat-affected zone (HAZ) on the G115 side after welding is 3.7 mm. After PWHT, dynamic recovery occurs in the FGHAZ of the G115 side. The precipitates increase, martensite laths are polygonal, dislocation density is reduced, residual austenite disappears. The FGHAZ with large residual stress after welding undergoes stress relaxation during PWHT. Residual stress in the FGHAZ is reduced, the dislocation density is reduced, which reduces the effect of dislocation strengthening and martensite lath strengthening. The strength of the FGHAZ is lowered than BM.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据