4.8 Article

A self-driven alloying/dealloying approach to nanostructuring micro-silicon for high-performance lithium-ion battery anodes

期刊

ENERGY STORAGE MATERIALS
卷 34, 期 -, 页码 768-777

出版社

ELSEVIER
DOI: 10.1016/j.ensm.2020.10.021

关键词

Self-driven alloying/dealloying; Molten salt; Silicon kerf waste; Silicon anode; Lithium-ion batteries

资金

  1. Fundamental Research Funds for the Central Universities [XLYC1807042]
  2. National Key R&D Program of China [N2025035, N2025034]
  3. 111 Project [2018YFC1901804]
  4. [B16009]

向作者/读者索取更多资源

The self-driven alloying/dealloying approach and vacuum-distillation process improve the utilization of micro-sized silicon, reduce the use of toxic reagents, and maintain a closed-loop material circle, offering an efficient and green pathway for enhancing lithium-storage anodes.
The nanostructuring of low-cost micro-sized silicon (mSi) is paramount to achieve the practical viability of deploying high-capacity Si anodes for lithium-ion batteries (LIBs). Conventional methods for converting mSi to nanoporous Si (nSi) involve low product yield, toxic chemical reagents, high energy consumption, etc. Herein, we report a self-driven alloying/dealloying approach to converting mSi to nSi in molten salts, where mSi alloys with Mg powders to generate Mg2Si and, subsequently, the Mg2Si dealloys in a Mg2Si parallel to Sn primary battery with the production of nSi at the negative electrode and the liquid Mg-Sn alloy at the positive electrode. Finally, the Mg-Sn decomposes to Mg gas and liquid Sn through a vacuum-distillation process. Taking the micro-sized Si kerf waste as an example, the pyrolytic carbon-coated (PCC) nSi delivers a capacity of 1080.2 mAh g(-1) at 1 A g(-1) after 1000 cycles with a capacity retention rate of 83.7%. Furthermore, a fabricated PCC-nSi-2 parallel to LiNi0.6Co0.2Mn0.2O2 (NCM622) full cell demonstrates a high energy density of 466 Wh kg(-1) as well as good cycling stability for 200 cycles. The improved Li-storage performance is attributed to the synergetic effects of the nanoporous Si and carbon coating. Overall, the self-driven nanostructuring approach along with the vacuum-distillation process maintains a high utilization of mSi, eliminates the use of toxic reagents, and keeps a closed-loop material circle, and thus offers an efficient and green pathway to valorize various mSi for making enhanced lithium-storage anodes.