4.7 Article

Nanowire-toughened transition layer to improve the oxidation resistance of SiC-MoSi2-ZrB2 coating for C/C composites

期刊

CORROSION SCIENCE
卷 111, 期 -, 页码 259-266

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.corsci.2016.05.013

关键词

Ceramic matrix composites; Weight loss; High temperature corrosion

资金

  1. National Natural Science Foundation of China [51221001, 51572223, 51222207]
  2. Research Fund of State Key Laboratory of Solidification Processing (NWPU), China [12-BZ-2014]
  3. 111 Project [B08040]

向作者/读者索取更多资源

To enhance the oxidation resistance of SiC-MoSi2-ZrB2 coating for C/C composites, pre-oxidation treatment and chemical vapor deposition were applied to construct a SiC nanowire-toughened inlaid transition layer between C/C and SiC-MoSi2-ZrB2 coating. The results show that the coating prepared with pre-oxidation and SiC nanowires has better oxidation resistance, which can protect C/C for 124 h at 1773 K in air with the weight loss per unit area of 1.1 mg cm(-2). The synergistic effect of the inlaid structure of the transition layer and SiC nanowires plays positive role on alleviating the mismatch of thermal expansion coefficient between C/C and SiC-MoSi2-ZrB2 coating. (C) 2016 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据