4.7 Article

New biodegradable nanoparticles-in-nanofibers based membranes for guided periodontal tissue and bone regeneration with enhanced antibacterial activity

期刊

JOURNAL OF ADVANCED RESEARCH
卷 28, 期 -, 页码 51-62

出版社

ELSEVIER
DOI: 10.1016/j.jare.2020.06.014

关键词

Nanoparticles; Nanofibers; GTR; GBR; Periodontal

向作者/读者索取更多资源

A new series of nanofibrous scaffolds were prepared in this study for GTR/GBR applications, with enhanced cell viability and antibacterial activity through the incorporation of hydroxyapatite nanoparticles and green-synthesized silver nanoparticles, respectively. The scaffolds showed a desirable degradation profile, losing around 40-70% of their mass in 8 weeks, making them promising for both GTR and GBR applications.
Introduction: Guided tissue regeneration (GTR) and guided bone regeneration (GBR) are commonly used surgical procedures for the repair of damaged periodontal tissues. These procedures include the use of a membrane as barrier to prevent soft tissue ingrowth and to create space for slowly regenerating periodontium and bone. Recent approaches involve the use of membranes/scaffolds based on resorbable materials. These materials provide the advantage of dissolving by time without the need of surgical intervention to remove the scaffolds. Objectives: This study aimed at preparing a new series of nanofibrous scaffolds for GTR/GBR applications with enhanced mechanical properties, cell adhesion, biocompatibility and antibacterial properties. Methods: Electrospun nanofibrous scaffolds based on polylactic acid/cellulose acetate (PLA/CA) or poly(caprolactone) (PCL) polymers were prepared and characterized. Different concentrations of green-synthesized silver nanoparticles, AgNPs (1-2% w/v) and hydroxyapatite nanoparticles, HANPs (10-20% w/v) were incorporated into the scaffolds to enhance the antibacterial and bone regeneration activity. Results: In-vitro studies showed that addition of HANPs improved the cell viability by around 50% for both types of nanofibrous scaffolds. The tensile properties were also improved through addition of 10% HANPs but deteriorated upon increasing the concentration to 20%. AgNPs significantly improved the antibacterial activity with 40 mm inhibition zone after 32 days. Additionally, the nanofibrous scaffolds showed a desirable degradation profile with losing around 40-70% of its mass in 8 weeks. Conclusions: The obtained results show that the developed nanofibrous membranes are promising scaffolds for both GTR and GBR applications. (C) 2021 The Authors. Published by Elsevier B.V. on behalf of Cairo University.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据