4.8 Article

Flux-free synthesis of single-crystal LiNi0.8Co0.1Mn0.1O2 boosts its electrochemical performance in lithium batteries

期刊

JOURNAL OF POWER SOURCES
卷 464, 期 -, 页码 -

出版社

ELSEVIER
DOI: 10.1016/j.jpowsour.2020.228207

关键词

Spray pyrolysis; Hybrid oxides; Flux-free; LiNO3; Single-crystal LiNi0.8Co0.1Mn0.1O2

资金

  1. Science and Technology Department of Guangxi Zhuang Autonomous Region [AD18281073]
  2. Government of Chongzuo, Guangxi Zhuang Autonomous Region [FA2019015]

向作者/读者索取更多资源

The single-crystal cathode materials exhibit better cyclic stability, enhanced compaction density, and improved safety than polycrystalline cathode materials. They, therefore, are ideal cathode material candidates for lithiumion batteries. Introducing hetero materials, excessive sintering temperature and tedious steps during the synthesis of the single-crystal cathode materials, however, limit their large-scale application. In this work, we adopt the spray pyrolysis method to prepare the hybrid oxides NiO-MnCo2O4-Ni6MnO8. This kind of hybrid oxides is considered to be an ideal precursor for the single-crystal Ni-rich cathode materials owing to its fine particle size and porous structure. Subsequently, high-temperature lithiation synthesises the submicron single-crystal LiNi0.8Co0.1Mn0.1O2 (NCM811) cathode material. The synthesis temperature of the submicron single-crystal NCM811 is significantly lowered when LiNO3 is selected as the lithium source and serves as the flux agent taking advantage of its fusibility. Consequently, the as-synthesized submicron single-crystal NCM811, compared with conventional polycrystalline NCM811, exhibits long lifetime applications, improved thermal stability and micro-crack immunity. The synthetic strategy in this work also demonstrates that the crystal crushing process, flux adding, and repeated sintering are not indispensable in the synthesis of single-crystal cathode materials.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.8
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据