Serpentinization and H2 production during an iron-clay interaction experiment at 90C under low CO2 pressure

期刊

APPLIED CLAY SCIENCE
卷 191, 期 -, 页码 -

出版社

ELSEVIER
DOI: 10.1016/j.clay.2020.105609

关键词

Serpentinization; Iron-clay interaction; Hydrothermal experiment; Corrosion; H-2; Geochemical modelling

资金

  1. Andra (French national agency for the management of radioactive waste)

向作者/读者索取更多资源

Interactions between steel canisters and clay-rich material in deep geological repositories for high-level nuclear waste were studied by reacting metallic iron and a claystone from the Callovo-Oxfordian formation of the Paris Basin (COx). The experiment ran at 90 degrees C for 14 weeks in the presence of water and under 20 mbar of initial CO2 partial pressure (p(CO2)). At the end of the experiment, the pressure in the autoclave reached 50 bar due to H-2 production. Water was almost entirely consumed and poorly crystallized 7 A-greenalite-type clays were formed at the expense of illite and mixed-layered illite-smectite minerals (I/S). The dissolution of quartz and pyrite and the crystallization of pyrrhotite were also observed. Considering the results of Mossbauer and Fourier Transformed Infrared (FTIR) spectroscopies, iron carbonate and and/or ferrous hydroxycarbonate were suspected to precipitate but in very small amounts. A follow-up of the mineralogical evolution by XRD (X-ray diffraction), SEM (Scanning Electron Microscopy) and TEM (Transmission Electron Microscopy) shows that serpentinization of clays (formation of greenalite) is accompanied by a significant consumption of water and the production of H-2 gas due to the oxidation and dissolution of metallic iron. Experimental results are in good agreement with geochemical modelling with the PHREEQC code. The kinetics of the iron corrosion was evaluated from H-2 production and shows that diffusion processes are the rate limiting step.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据