Insight on esterase from Pseudomonas aeruginosa strain S3 that depolymerize poly(lactic acid) (PLA) at ambient temperature

期刊

POLYMER DEGRADATION AND STABILITY
卷 174, 期 -, 页码 -

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.polymdegradstab.2020.109096

关键词

Pseudomonas aeruginosa; PLA; Biodegradation; Esterase; Plackett-burman design; Central composite design; LCMS

向作者/读者索取更多资源

Pseudomonas aeruginosa strain S3 exhibited high esterolytic activity against poly (lactic acid) (PLA) at environmental temperature (similar to 30 degrees C). A comprehensive study was conducted for optimization of physicochemical parameters for high-throughput esterase production using Plackett-Burman Design and Central Composite Design. PLA degradation by Pseudomonas aeruginosa strain S3 was confirmed during preliminary studies using Fourier Transform Infrared Spectroscopy (FTIR) and scanning electron microscopy (SEM). The date obtained from statistical optimization demonstrated interactive action of inoculum size with peptone, yeast extract and Tween 20 was more influential towards esterase activity. The following medium constituents were optimized for maximum esterase production [(g/L) Glucose, 0.8; Peptone, 10.5; Yeast extract, 15; MgSO4.7H(2)O, 0.3; Sodium citrate, 4; CaCl2, 1; NaCI, 1; FeSO4.7H(2)O, 1; Inoculum size 75 mL and Tween 20, 3.8 mL (v/v)]. The molecular weight of purified esterase was approximately 35 kDa with apparent K-m and V(max )values, i.e., K-m 12.38 mu M and V-max 769.23 U/mg, respectively. The enzyme showed stability over a broad range of pH (3-10) and temperature (20-40 degrees C). The activity of the purified enzyme was significantly enhanced by non-polar detergents (Tween 80 and Triton-X100), glycerol as well as both mono and divalent cations (Co+2 and K+1). Hydrolysis of PLA films with purified esterase released oligomers of medium chain length (n = 6-13), reaffirming the biodegradation potential of Pseudomonas aeruginosa strain S3 against PLA. The results obtained from the study demonstrate the potential of our strain and its enzymes in development of high efficient system of PLA biodegradation and recovery processes. (C) 2020 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据