{10(1)over-bar2} twinning behavior under biaxial tension of Mg-3Al-1Zn plate

期刊

INTERNATIONAL JOURNAL OF PLASTICITY
卷 132, 期 -, 页码 -

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.ijplas.2020.102754

关键词

Magnesium alloy; Twinning; Biaxial tension; Mechanical behavior

资金

  1. Natural Science Foundation of China [51871032, 51421001]
  2. Fundamental Research Funds for the Central Universities [2019CDQYCL032]
  3. 111 Project under the Ministry of Education [B16007]

向作者/读者索取更多资源

Although {10 (1) over bar2} twinning behavior has been extensively studied, it has rarely been investigated under biaxial tension. In the present research, the mechanical response and {10 (1) over bar2} twinning behavior of a Mg AZ31 sheet under biaxial tension with various stress ratios (sigma(ND) : sigma(TD)) along the normal direction (ND) and transverse direction (TD) were systematically studied. The results indicate that the yield stress along the ND is nearly independent of sigma(ND) : sigma(TD). Schmid law applied to {10 (1) over bar2} twinning under biaxial tension yields better efficiency than that for uniaxial tension, and a higher efficiency is observed with a larger stress ratio along the TD; the fraction of experimentally observed twin variants with Schmid factors (SFs) of ranks 1 and 2 is approximately 45% for uniaxial tension, whereas it is approximately 68% for sigma(ND) : sigma(TD) = 2 : 1 and approximately 88% for sigma(ND) : sigma(TD) = 1 : 2. This result contradicts with the previously reported result that Schmid law is more efficient for uniaxial stress states than under multiaxial stress conditions. It is found that biaxial tension will increase the difference in SF for the six twin variants and make Schmid law more efficient. Twin variant selection and volume fraction are highly dependent on sigma(ND) : sigma(TD). For uniaxial tension, the activities for the six variants are similar, and the (0002) poles of the twins are distributed evenly on a circle approximately 80 degrees-90 degrees away from the ND. In contrast, the variants (0 (1) over bar 12) [01 (1) over bar1] and (01 (1) over bar2) [0 (1) over bar 11] are more favorable under biaxial tension, and more (0002) poles of the twins concentrate around the rolling direction with a higher ratio of sigma(TD). At a similar strain level, the twin fraction under biaxial tension is often different from that under uniaxial tension, and this difference varies with sigma(ND): sigma(TD). This mechanism is associated with a stress-ratio-mediated detwinning behavior under biaxial tension. The findings in the present study provide a new and significant understanding of the twinning behavior of Mg alloys.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据