Y3Al5O12:Ce3+, Gd3+(YAG:Ce3+, Gd3+) phosphors were synthesized by a high-energy ball milling method. The X-ray diffraction (XRD) patterns showed their garnet structure, and several diffraction peaks shifted to lower angle side when co-doped with Gd3+ ions. Field emission scanning electron microscopy images exhibited irregular spherical particles of about 2 mu m size. The photoluminescence (PL) properties of the YAG:Ce3+, Gd3+ phosphors were studied as a function of the Gd3+ ion concentration. The PL excitation (PLE) spectra exhibited the broadband 4f-5d transition of Ce3+ ions centered at 439 nm. The PL spectra showed the intense 5d-4f transition of the Ce3+ ions with a band maximum at 542 nm, and this band maximum shifted to the longer wavelength region by increasing concentration of the Gd3+ ion. (C) 2015 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据