期刊
CERAMICS INTERNATIONAL
卷 42, 期 6, 页码 7819-7823出版社
ELSEVIER SCI LTD
DOI: 10.1016/j.ceramint.2016.02.013
关键词
Grain growth; Yttria; Transparent ceramic; SPS
Yttria nanopowder was used to fabricate transparent yttria ceramics by spark plasma sintering at temperatures ranging from 1200 degrees C to 1600 degrees C for 20 min. The microstructure of fracture cross section and optical transmittance of the products were characterized by Field Emission -Scanning Electron Microscope (FE-SEM) and Fourier-transform infrared spectrophotometer (FTIR). With increasing the sintering temperature, densification occurs up to 1500 degrees C, whereas the mean grain size of yttria ceramics was first increased and then decreased markedly. The highest density and the lowest mean grain size of yttria ceramic reached to 99.58% and 0.53 mu m at 1500 degrees C, respectively. The best in-line transmittance was at 1500 degrees C, with transmittance being about 80% in the range of 3-5 mu m, which was close to the theoretical value of yttria. (C) 2016 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据