4.6 Article

Hydrophilic and Superhydrophilic Self-Cleaning Coatings by Morphologically Varying ZnO Microstructures for Photovoltaic and Glazing Applications

期刊

ACS OMEGA
卷 5, 期 2, 页码 1033-1039

出版社

AMER CHEMICAL SOC
DOI: 10.1021/acsomega.9b02758

关键词

-

资金

  1. RCUK's Energy Programme [EP/P003605/1]
  2. EPSRC IAA Grant [EP/R511699/1]
  3. EPSRC [EP/P003605/1] Funding Source: UKRI

向作者/读者索取更多资源

Transparent, superhydrophilic materials are indispensable for their self-cleaning function, which has become an increasingly popular research topic, particularly in photovoltaic (PV) applications. Here, we report hydrophilic and superhydrophilic ZnO by varying the morphology for use as a self-cleaning coating for PV applications. Three different ZnO microstructures, such as ZnO nanorods (R-ZnO), ZnO microflowers (F-ZnO), and ZnO microspheres (M-ZnO), were developed by hydrothermal methods. The surface morphology by using X-ray diffraction (XRD), wettability behavior by using water contact angle (WCA) measurements, structural and optical properties by using photoluminescence (PL), Raman, and UV-vis spectrophotometry, and defect estimation by using X-ray photoelectron spectroscopy (XPS) of the ZnO nanostructured films were systematically investigated. XRD confirmed the formation of the hexagonal wurtzite structure of ZnO. The average crystallite sizes of prepared R-ZnO, F-ZnO, and M-ZnO were found to be 28.95, 11.19, and 41.5 nm, respectively. The band gap values of ZnO nanostructures were calculated from the UV-vis absorption spectrum and found to be 3.6, 3.3, and 3.1 eV for R-ZnO, F-ZnO, and M-ZnO, respectively. The WCAs for R-ZnO and F-ZnO were 20.2 and 11.19 degrees, respectively, while M-ZnO behaved like a superhydrophilic material having a WCA of 2.8 degrees.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据