4.7 Article

Fluoroalkyl Pentacarbonylmanganese(I) Complexes as Initiators for the Radical (co)Polymerization of Fluoromonomers

期刊

POLYMERS
卷 12, 期 2, 页码 -

出版社

MDPI
DOI: 10.3390/polym12020384

关键词

fluoropolymers; manganese complexes; nuclear magnetic resonance; radicals; organometallic-mediated radical polymerization; vinylidene fluoride

资金

  1. Agence Nationale de la Recherche (ANR, French National Agency) [ANR-14-CE07-0012]
  2. Centre National de la Recherche Scientifique (CNRS)

向作者/读者索取更多资源

The use of [Mn(R-F)(CO)(5)] (R-F = CF3, CHF2, CH2CF3, COCF2CH3) to initiate the radical polymerization of vinylidene fluoride (F2C=CH2, VDF) and the radical alternating copolymerization of vinyl acetate (CH2=CHOOCCH3, VAc) with tert-butyl 2-(trifluoromethyl)acrylate (MAF-TBE) by generating primary R-F(center dot) radicals is presented. Three different initiating methods with [Mn(CF3)(CO)(5)] (thermal at ca. 100 degrees C, visible light and UV irradiations) are described and compared. Fair (60%) to satisfactory (74%) polyvinylidene fluoride (PVDF) yields were obtained from the visible light and UV activations, respectively. Molar masses of PVDF reaching 53,000 gmol(-1) were produced from the visible light initiation after 4 h. However, the use of [Mn(CHF2)(CO)(5)] and [Mn(CH2CF3)(CO)(5)] as radical initiators produced PVDF in a very low yield (0 to 7%) by both thermal and photochemical initiations, while [Mn(COCF2CH3)(CO)(5)] led to the formation of PVDF in a moderate yield (7% to 23%). Nevertheless, complexes [Mn(CH2CF3)(CO)(5)] and [Mn(COCHF2)(CO)(5)] efficiently initiated the alternating VAc/MAF-TBE copolymerization. All synthesized polymers were characterized by H-1 and F-19 NMR spectroscopy, which proves the formation of the expected PVDF or poly(VAc-alt-MAF-TBE) and showing the chaining defects and the end-groups in the case of PVDF. The kinetics of VDF homopolymerization showed a linear ln[M](0)/[M] versus time relationship, but a decrease of molar masses vs. VDF conversion was noted in all cases, which shows the absence of control. These PVDFs were rather thermally stable in air (up to 410 degrees C), especially for those having the highest molar masses. The melting points ranged from 164 to 175 degrees C while the degree of crystallinity varied from 44% to 53%.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据