The thermal cracking of cotton stalks (CS) through pyrolysis was undertaken using a laboratory scale batch pyrolysis reactor. The distribution of pyrolysis products were studied dependent on the final pyrolysis temperature which ranged from 300 to 800 degrees C by 100K intervals. The maximum biochar yield of 46.5% was obtained at 400 degrees C. As the pyrolysis process temperature increased, the solid char product yield decreased. The largest higher heating value (25.845 MJ kg(-1)) was obtained at 600 degrees C. All biochar samples produced between 500 and 700 degrees C had an energy densification ratio of 1.41, indicating a higher mass-energy density than the initial feedstock. A larger share of syngas and bio-oil were produced at higher temperatures, as estimated. Preferential selection of a char based on the energy yield would lead to a selection of the 400 degrees C product, while selection based on the energy densification ratio would be for a product obtained between 500 and 700 degrees C. An energy simulation was conducted which determined that the process is self-sustaining at and above 400 degrees C. Furthermore, the global energy potential was determined from CS pyrolysis, which was estimated at 380 PJ yr(-1) could contribute to roughly 0.1% of the actual global total primary energy supply of 576 EJ yr(-1). (C) 2019 Elsevier Ltd. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据