4.4 Article

Observation of Variations in Condensed Carbon Morphology Dependent on Composition B Detonation Conditions

期刊

PROPELLANTS EXPLOSIVES PYROTECHNICS
卷 45, 期 2, 页码 347-355

出版社

WILEY-V C H VERLAG GMBH
DOI: 10.1002/prep.201900213

关键词

Detonation nanodiamond; composition B; small-angle x-ray scattering; transmission electron microscopy; thermochemical modeling

资金

  1. LLNL LDRD [14-ERD-018]
  2. NNSA Office of Defense and Nuclear Nonproliferation
  3. NNSA Science Campaign 2
  4. U.S. Department of Energy (DOE) [DE-AC52-07NA27344]
  5. U.S. DOE NNSA award [DE-NA0002442]
  6. U.S. DOE Office of Science User Facility [DE-AC02-06CH11357]
  7. DOE Office of Science User Facility [DE-AC02-05CH11231]
  8. Lawrence Fellowship [LLNL-JRNL-778657]

向作者/读者索取更多资源

Carbon particulates generated during detonation depend upon high explosive type, composition, and detonation conditions. Although explosive composition greatly affects particulates, the focus of this work is on how detonation geometries that induce much higher temperatures and pressures in the high explosive lead to differing particulate morphologies. In this study, two geometries were used: Detonations were initiated in Composition B cylinders at one end in conventional detonations and initiated at both ends to produce colliding detonations. Each of these detonations was observed on the sub-mu s timescale using fast radiography capturing images of the front moving through the cylinder, and colliding detonation fronts in real-time. These imaging experiments were complemented with time-resolved small-angle x-ray scattering (SAXS) experiments that were able to observe and determine the varying condensed carbon morphologies at different locations and times in each detonation. The detonations could be timed in such a way that the spatial and temporal dependence of the carbon morphology could be superimposed onto radiography images collected at the same point in time. The complementary approach is able to show that the carbon condensates are much larger when formed in the elevated temperature and pressure conditions near the location of colliding detonation fronts. Thermochemical modeling suggests that these larger particulates form either in the diamond phase or on the liquidus line of the carbon phase diagram. The increase in size observed by SAXS may correlate well with the increased residence time deeply in the diamond phase. These particulates can be described as nano-sized phases with some surface texture or otherwise near-surface intra-particle heterogeneity.