4.7 Article

CaCO3 mineralization in polymer composites with cellulose nanocrystals providing a chiral nematic mesomorphic structure

期刊

出版社

ELSEVIER
DOI: 10.1016/j.ijbiomac.2019.09.045

关键词

Cellulose nanocrystal; Chiral nematic liquid crystal; Polymer composites; Calcium carbonate mineralization

资金

  1. Japan Society for the Promotion of Science (JSPS) [17K15295, 26252025]
  2. Grants-in-Aid for Scientific Research [17K15295] Funding Source: KAKEN

向作者/读者索取更多资源

CaCO3 mineralization was carried out using cellulose nanocrystal (CNC)/polymer composites wherein a chiral nematic structure of CNC assembly was immobilized in advance via a polymerization process of the precursory aqueous CNC/vinyl monomer lyotropics (7-11 wt% CNC in feed). Two series of polymer composites were prepared: CNC/poly(2-hydroxyethyl methacrylate) (PHEMA) and CNC/poly(2-hydroxyethyl methacrylate-co-acrylic acid) (P(HEMA-co-AA), HEMA:AA = 95:5-70:30 in mol). The mineralization was allowed to proceed solely by soaking the composite films in a salt solution containing Ca2+ and HCO3- under a low-basic condition (pH 9). Polymorphism of CaCO3 deposited inside the films was examined by X-ray diffractometry as a function of the soaking time (1-5 day) and also of the matrix composition. In the CNC/PHEMA series, the polymorphic form changed from amorphous calcium carbonate (ACC) (1-day soaking) to metastable crystalline vaterite (3-day soaking) and then to a mixture of vaterite and aragonite (5-day soaking). In the mineralization of the CNC/P(HEMA-co-AA) series, the formation of stable calcite was prominent besides minor appearance of vaterite. It was deduced that the mesofiller CNC and the AA unit in the vinyl polymer, both bearing an anionic group (-SO3- or -COO-), contributed to capturing Ca2+ to facilitate the CaCO3 deposition in the swollen film matrix. The pre-invested chiral nematic organization was kept in any of the mineralized films (dried); however, the helical pitch was appreciably reduced relative to that observed before the mineralization, attributable to the increase of ionic strength in the CNCs' surroundings accompanied by the wet process. Thermogravimetry showed that the mineralization definitely improved the thermal performance (heat/flame resistance) of the mesomorphic order-retaining CNC/polymer composites. (C) 2019 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据