The present study focuses on the design and fabrication of passive solar still system with phase change materials (PCM). In order to improve the distillate, PCMs (paraffin wax, stearic acid, and lauric acid) have been stored in a copper cylinder. The effects of basin water depth on total distillate have been studied for all three cases. The maximum distillate has been obtained at 1 cm depth for all cases with three PCMs used in this study. Total distillate decreased linearly with water depth for all three PCMs. There has been a 9.2% drop in the maximum water basin temperature in paraffin wax as compared to stearic acid (17.6%) and lauric acid (21.5%) with an increase in water depth from 1 to 5 cm. Heat transfer and energy balance equations involved in the present solar still system have been stated. Variation of some heat transfer coefficients with time has also been studied for three different PCMs. The total distillate has been found to be increased by 1202, 1015, and 930 ml/m(2)-day for paraffin wax, stearic acid, and lauric acid, respectively stored in a copper cylinder. The performance of lauric acid for total distillate has been comparable with the other two PCMs. (C) 2019 The Authors. Published by Elsevier Ltd.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据