Interaction between iron ore and magnesium additives during induration process of pellets

期刊

POWDER TECHNOLOGY
卷 361, 期 -, 页码 894-902

出版社

ELSEVIER
DOI: 10.1016/j.powtec.2019.11.006

关键词

Iron ore; Magnesium olivine; Magnesia fines; Induration process; Interaction mechanism

资金

  1. National Natural Science Foundation of China [51874025]
  2. National Key Research and Development Program of China [2017YFB0304300, 2017YFB0304302]

向作者/读者索取更多资源

To eliminate the adverse effect of incompletely mineralized magnesium additive on pellets strength, clarify the interaction between additives and iron ore during the induration process, two types of interaction couples were prepared and scanning electron microscopy-Energy dispersive spectrometer was used to study the diffusion of elements and phase transformation during the induration. Results show that the diffusion of Mg dominates both interactions. The diffusion of Fe from ore to magnesia fines and magnesium olivine are accompanied by the migration of Si, the former generates Magnesioferrite and Forsterite while the latter also generates Fayalite. For the diffusion of Mg from magnesia fines to ore, Mg only reacts with iron oxides and forms Magnesioferrite, but in the ore-olivine couple, Mg both diffuses into iron oxides and silicate, which indicates that the reaction mechanism of two couples is different. The interaction schematic diagrams of each couple are given in this paper. (C) 2019 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据