4.2 Article

Morphological and transport characteristics of swollen chitosan-based proton exchange membranes studied by molecular modeling

期刊

BIOPOLYMERS
卷 107, 期 1, 页码 5-19

出版社

WILEY
DOI: 10.1002/bip.22979

关键词

chitosan biopolymer; methanol; molecular modeling; proton exchange membrane

资金

  1. Golestan University (GU)

向作者/读者索取更多资源

Chitosan biopolymer has been extensively applied in direct methanol fuel cells (DMFCs) as a potential replacement to conventional Nafion membrane for its considerably reduced methanol crossover. Here, we computationally explored the influences of methanol concentration, temperature, and pH parameters upon the nanostructure and dynamics, particularly the methanol crossover, in chitosan proton-exchange membrane (PEM) through molecular dynamics simulations. Theoretical results demonstrated the increased swelling and radius of gyration of chitosan chains at higher concentrations. Structural examinations further revealed that an increase in methanol loading weakened the water interactions with chitosan functionalities (amineNH(2), hydroxylOH, and methoxyCH(2)OH) whereas improved the methanol affinities toward chitosan, reflecting higher methanol sorption capability of chitosan at enhanced concentrations. Additionally, it was found that interactions between solvents and chitosan strengthened under acidic pH conditions on account of amine protonation. The water diffusivity inside the swollen chitosan diminished by increasing CH3OH uptake, and in contrast diffusivity of methanol was noted to enhance. Furthermore, it was observed that an enhancement in temperature or a decrease in pH intensified solvent mobility. These insights imply that supplying methanol-concentrated and/or acidic feed solutions into DMFCs based on chitosan PEMs could lower membrane performance due to the significant methanol transport dynamics.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.2
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据