4.7 Article

Experimental analysis on the degradation behavior of overdischarged lithium-ion battery combined with the effect of high-temperature environment

期刊

INTERNATIONAL JOURNAL OF ENERGY RESEARCH
卷 44, 期 1, 页码 229-241

出版社

WILEY
DOI: 10.1002/er.4898

关键词

degradation; high temperature; lithium-ion battery; overdischarge

资金

  1. National Key R&D Program of China [2018YFC0808600]

向作者/读者索取更多资源

A set of experiments are performed in the present work to investigate the degradation behavior of lithium-ion battery during overdischarge cycling, as well as the influence of a high-temperature environment on the degradation. Among, different discharge cut-off voltages (1.0, 0.5, and 0.2 V) are included. During the overdischarge process, batteries experience a stage where a violent electro-thermal behavior is exhibited, involving sharp decreases in the voltage and current, and a fierce increase in the surface temperature; moreover, several parameters such as the discharge capacity, energy density, and internal resistances are all increased after overdischarge. Besides, a poor rate capacity and serious capacity degradation can also be seen during the overdischarge cycling, which is further reflected by the evolution of battery surface temperature, charge/discharge voltage, and internal resistances. What is more, it is found that battery electro-thermal parameters, eg, temperature rise, degradation rate, and internal resistances, increase exponentially as overdischarge deepens. Finally, a high-temperature environment is verified to deteriorate the degradation of overdischarged battery.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据