In-depth study of annealed porous silicon: Understand the morphological properties effect on negative LiB electrode performance

期刊

ELECTROCHIMICA ACTA
卷 323, 期 -, 页码 -

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.electacta.2019.134758

关键词

-

资金

  1. National Agency for Research under the program Investments for future [ANR-10-LABX-05-01]

向作者/读者索取更多资源

Silicon (Si) used as negative electrode in a Li-ion battery (LIB) is highly attractive for its high energy density, safe cycling, and nontoxicity. However its alloying mechanism with Li induces material pulverization, which leads to a rapid capacity fade. In this work, annealing post treatment was used in order to tune the morphological properties of porous silicon. Playing on annealing temperature, the morphological modification induces electrochemical behavior changes in LIB. The porosification is an interesting way to accommodate the volume expansion occurring during the alloying process. Increase of the annealing temperature leads to porous Si pores and walls reorganization, which has a positive impact on battery performance likely due to a higher wettability of the Si electrode with electrolyte. 700 degrees C appeared to be the optimized annealing temperature. (C) 2019 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据