4.7 Article

Plastic anisotropy and deformation-induced phase transformation of additive manufactured stainless steel

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/j.msea.2019.138065

关键词

Additive manufacturing; Stainless steel; Anisotropy; Phase transformation; Neutron diffraction

资金

  1. National Research Foundation - Korean government [2016R1A2B4015701, 2017K1A3A7A09016308]
  2. Ministry of Science and Technology Programs [107-2628-E-009-001-MY3, 107-2218-E-009-003]
  3. National Synchrotron Radiation Research Center (NSRRC) Neutron Program
  4. National Research Foundation of Korea [2016R1A2B4015701] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)

向作者/读者索取更多资源

Plastic anisotropy and deformation-induced phase transformation of additively manufactured (AM) stainless steels were investigated via in-situ neutron diffraction, electron backscatter diffraction, metallography, and fractography. Two types of tensile specimens were manufactured: (1) One sample was vertically fabricated with its tensile axis parallel to the z-direction (AM-V), (2) The other sample was horizontally fabricated with its tensile axis perpendicular to the z-direction (AM-H). A commercial 15-5PH stainless steel (CA) was used for comparison. AM steel revealed enhanced yield strength, tensile strength, and uniform elongation over CA, which was mainly due to grain refinement and transformation induced plasticity (TRIP). Different onsets of strain nonlinearity between AM-V and AM-H were closely related to martensitic phase transformation. Stresses estimated from lattice strains measured by neutron diffraction matched well with the applied stress-strain curves. After plastic deformation, voids were formed and congregated near the solidified line where fine grains were populated. Higher dislocation density was observed in the fine grain zone, and lower density was shown in the relatively coarse grain zone. AM steels exhibited significant anisotropic fracture behavior in terms of loading direction. In contrast to isotropic failure for CA and AM-V, AM-H revealed anisotropic failure with elliptical formation of the fracture feature. The fracture surface of AM-H possessed many secondary cracks propagating perpendicular to the building direction. The occurrence of secondary cracks in AM-H resulted in rapid load drop during tensile loading after necking.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据