4.3 Article

Comparison between wet and dry timber visual strength grading according to the Spanish (UNE 56544) and German (DIN 4074-1) standards

期刊

MATERIALES DE CONSTRUCCION
卷 69, 期 336, 页码 -

出版社

CONSEJO SUPERIOR INVESTIGACIONES CIENTIFICAS-CSIC
DOI: 10.3989/mc.2019.03319

关键词

Wood; Detection of cracks; Mechanical properties; Modulus of elasticity; Dry grading

资金

  1. Ministerio de Economia y Competitividad [Spanish Ministry of Economy and Competitiveness] [BIA 2014-55089-P, BIA 2010-18858]

向作者/读者索取更多资源

Visual strength grading is widely used to estimate mechanical properties of structural timber. National visual grades are allocated to strength classes according to European standard EN1912. The recent discussion about the proper function of visual strength grading standards and the assignment of strength classes shows the need for further research in this field. Spanish-sourced radiata, Scots, Salzmann and maritime pine timber samples were visually graded in wet and dry condition according to the Spanish UNE56544 (2011) and German DIN4074-1 (2012) standards. Rejection was far higher dry due to distortion (warping) parameters. However, this rejection could be significantly mitigated by adopting a higher twist limit (2 mm / 25 mm width). UNE 56544 is more suitable for visually grading these species because it was specifically designed for them and a Spanish source. However, both standards underestimated the Scots pine rejection pieces which mechanical properties fulfill the MEG and S10 grades.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据