The goal of this work was to investigate biophysical stability of iron-pectin nanoparticles and analyze the feasibility of using them as delivery systems for the probiotic strain Lactobacillus plantar= CIDCA 83114. Iron oxide (Fe3O4) nanoparticles were synthesized from 0.25M FeCl2/0.5 M FeCl(3)6H(2)O, and coated with citrus pectins. Their physico-chemical properties [MR, X-ray diffraction (XRD), zeta-potential, particle size, SEM, TEM] and their effect on bacterial stabilization (viability after freeze-drying/storage, stability when exposed to simulated gastrointestinal conditions) were assessed. XRD indicated the almost exclusive presence of magnetite crystalline phases. FTIR spectra confirmed the adsorption of pectin on magnetite nanoparticles surface. SEM and TEM images evidenced agglomerated nanoparticles, and a morphological surface change after adsorption of pectin. DLS and zeta-potential results proved the solvation of the ionizable groups in the hydrophilic network which induced chain expansion and agglomeration. Iron from nanoparticles demonstrated to be non-toxic for microorganisms up to 1.00 mg/mL. Simulated saliva and gastric solutions prevented nanoparticles from dissolution. The higher pH of the intestinal conditions (solvated -COO- and Fe-O- groups) facilitated the dispersion and partial dissolution of nanoparticles. Pectins adsorption on magnetite nanoparticles significantly enhanced electrostatic repulsion, which aided the solvation of ionized iron forms. The soluble species diffused out from the aggregates, being detected in the simulated intestinal fluid. Regarding bacterial viability, no decays were observed neither when pectin-decorated nanoparticles were exposed to simulated fluids nor when stored at 4 degrees C for 60 days. The composites engineered in this work appear as adequate delivery systems for probiotic bacteria, whose target is the gut.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据