Assessing the impact of small amounts of water and iron oxides on adhesion in the wheel/rail interface using High Pressure Torsion testing

期刊

TRIBOLOGY INTERNATIONAL
卷 135, 期 -, 页码 55-64

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.triboint.2019.02.024

关键词

Wet rail; Low adhesion; Wheel/rail interface; Water

资金

  1. Rail Safety and Standards Board (RSSB)
  2. Network Rail [T1077]

向作者/读者索取更多资源

A new High Pressure Torsion (HPT) set-up has been developed for assessing the effect of third body materials in the wheel/rail interface in a representative and controlled manner. In this study the technique has been used to investigate the effect of small amounts of water and iron oxides mixtures when subjected to different contact pressures. HPT tests showed reduction in adhesion relative to a dry contact when testing with small amounts of water and/or oxides, however sustained low adhesion (mu < 0.05) was not produced. To aid interpretation of the results a model has been developed to explore the behavior encountered when testing with water and iron oxide mixtures. The model relates the shear properties of water and oxide mixtures (with increasing solid content) to a predicted adhesion. The model shows a narrow window of water to oxide fraction is required for reduced adhesion, particularly on rough surfaces, and this correlates with the behavior observed.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据