Suppressed secondary phase generation in thermoelectric higher manganese silicide by fabrication process optimization

期刊

CERAMICS INTERNATIONAL
卷 45, 期 15, 页码 19538-19541

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.ceramint.2019.06.104

关键词

Thermoelectricity; Higher manganese silicide; Secondary phase; Solid-state reaction; Arc melting

资金

  1. National Research Foundation of Korea (NRF) Grant [2017R1A2A1A17069528]
  2. Priority Research Centers Program [2019R1A6A1A11055660]
  3. National Research Foundation of Korea [2017R1A2A1A17069528] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)

向作者/读者索取更多资源

Controlling the generation of secondary phases in thermoelectric higher manganese silicides is crucial to enhance their thermoelectric performance for use in automotive thermoelectric generators. However, the effect of different synthesis and sintering procedures on the secondary phase formation and thermoelectric properties has not yet been investigated. In this study, we demonstrate that fabricating Mn11Si19 via arc melting and spark plasma sintering results in a figure of merit (ZT) of 0.43 at 823 K, which is 15% higher than for a sample fabricated by a solid-state reaction and spark plasma sintering. We found that the presence of secondary MnSi phases in the Mn(11)Sin(19) samples was significantly reduced when using arc melting instead of solid-state reaction, which suggests that the phase formation behavior could be controlled by optimizing the fabrication process.