In this study, p-aramid (Kevlar) fabrics were impregnated with silica and silica-halloysite nanotube based shear thickening fluids to improve the impact resistance performance. Shear thickening fluids (STF) were synthesized using spherical silica particles of 100 nm diameter. Two virgin STF were prepared using silica concentrations of 60% and 65% (w/w). Then, halloysite nanotube (Hal nanotube) compounded STF were synthesized by adding Hal nanotube of 0.05, 0.1, 0.2 and 0.5% (w/w) with the existing STF. Rheological study confirmed more intense shear thickening behavior in silica-Hal nanotube compounded STF. Impact resistance of p-aramid fabrics increased drastically after the impregnation with STF. Further improvement in impact resistance was observed after silica-Hal nanotube compounded SIT impregnation. (C) 2016 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据