L1(2)-type Ni3Al alloys containing vanadium are potential candidates for solid-solution and age-hardenable alloy systems, according to the Ni3Al-Ni3V pseudo-binary phase diagram. Therefore, herein, variations in the microstructure and mechanical properties of Ni-13 at.% Al-12 at.% V-50 ppm B alloy during isothermal aging were investigated. Alloy specimens were solution-treated at 1323 K for 48 h, quenched in water, and aged at 1073 K to 1173 K. The quenched specimens exhibited a single phase of Ni3Al (L1(2) structure derived from Al (fcc) structure), while in the aged specimens, numerous fine disk-shaped precipitates identified as Ni3V (D0(22) structure from orthorhombic structure) were formed on {001} planes of the Ni3Al matrix. The size of the disk-shaped Ni3V precipitates increased gradually with increasing aging period. The hardness and strength of the specimens increased initially during aging at 1073 K to 1173 K, reached a maximum, followed by a subsequent decrease. The age-hardening behavior observed for the specimens can be explained in terms of precipitation of the fine disk-shaped Ni3V precipitates in the Ni3Al matrix. Furthermore, the peak-aged specimens exhibited an increase in yield strength with increasing testing temperature, similar to other L1(2)-type intermetallic alloys.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据