- European Regional Development Fund [01.2.2-LMT-K-718]
Several types of polyaniline (PANI) and polypyrrole (Ppy) nanocomposites with embedded glucose oxidase (GOx) and gold nanoparticles (AuNPs) were formed by enzymatic polymerization of corresponding monomers (aniline and pyrrole) in the presence of 6 and 13 nm diameter colloidal gold nanoparticles (AuNPs((6nm)) or AuNPs((13nm)), respectively) or chloroaurate ions (AuCl4-). Glucose oxidase in the presence of glucose generated H2O2, which acted as initiator of polymerization reaction. The influence of polymerization bulk composition and pH on the formation of PANI- and Ppy-based nanocomposites was investigated spectrophotometrically. The highest formation rate of PANI- and Ppy-based nanocomposites with embedded glucose oxidase and gold nanoparticles (PANI/AuNPs-GOx and Ppy/AuNPs-GOx, respectively) was observed in the solution of sodium acetate buffer, pH 6.0. It was determined that the presence of AuNPs or AuCl4- ions facilitate enzymatic polymerization of aniline and pyrrole.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据