4.7 Article

How changes in molecular weight and PDI of a polymer in amorphous solid dispersions impact dissolution performance

期刊

INTERNATIONAL JOURNAL OF PHARMACEUTICS
卷 556, 期 -, 页码 372-382

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.ijpharm.2018.12.012

关键词

Amorphous solid dispersion; Molecular weight; Polymer degradation; Multi-angle light scattering; Hot-melt extrusion; PVP-VA64

向作者/读者索取更多资源

Polymers functionally contribute to supersaturation and precipitation inhibition of the active pharmaceutical ingredient (API) in amorphous solid dispersions (ASD). Therefore, it is necessary to monitor physicochemical changes of the polymeric carrier caused by the manufacturing process. This is especially important when the material is exposed to heat and shear stress as in case of hot-melt extrusion (HME). This study evaluated the impact of HME process conditions on physical characteristics of poly(vinylpyrrolidone-co-vinyl-acetate) 60:40 (PVP-VA64) which is a widely used polymer for HME. Focus was set on molecular weight (M-w) and polydispersity index (PDI), by means of absolute molar mass detection via multi-angle light scattering. The generation of a high M-w fraction together with a decrease of the average M-w was detected. In a next step, the influence of these changes on the dissolution behavior of ASD was evaluated. Different stress conditions were applied onto PVP-VA64 in placebo extrusions. The obtained stressed polymer samples were subsequently used to prepare verum ASD with ketoconazole by spray drying (SD). SD dispersions (SDD) of thermally stressed PVPVA64 were compared to SDD prepared with bulk powder. Although there were only slight changes in M-w and PDI, they significantly impacted supersaturation and precipitation of the formulation.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据