4.4 Article

Thermoelectric Properties and Chemical Potential Tuning by K- and Se-Coalloying in (Pb0.5Sn0.5)1-xKxTe0.95Se0.05

期刊

ELECTRONIC MATERIALS LETTERS
卷 15, 期 3, 页码 342-349

出版社

KOREAN INST METALS MATERIALS
DOI: 10.1007/s13391-019-00130-1

关键词

Topological crystalline insulator; Dirac semimetal; Thermoelectric; ZT; Nano precipitation

资金

  1. National Research Foundation of Korea (NRF) - Ministry of Education, Science and Technology [2011-0030147]
  2. Materials and Components Technology Development Program of MOTIE/KEIT [10063286]
  3. National Research Foundation of Korea (NRF) - Korean Government(MSIP) [NRF-2015R1A5A1036133]

向作者/读者索取更多资源

Topological crystal insulator (TCI) and topological Dirac semimetals have topologically nontrivial surface and bulk state, respectively. The parent compound of Pb0.5Sn0.5Te exhibiting TCI band inversion has particle-hole symmetry owing to the gapless Dirac band implying a strong electron-hole bipolar compensation in Seebeck coefficient. We recently reported that weak perturbation of TCI state can enhance thermoelectric performance significantly due to highly dispersive and degenerated energy bands. It is a great interest that the further increase of chemical potential has beneficiary to thermoelectric performance in the vicinity of topological phase transition. Here we investigate the thermoelectric properties of the co-doping effect by K and Se in (Pb0.5Sn0.5)(1-x)KxTe0.95Se0.05 (x=0.0, 0.005, 0.010, 0.015, 0.02) compounds. K-doping increases the band gap from 0.15eV (Pb0.5Sn0.5Te) to 0.21eV (x=0.05) as well as increasing chemical potential resulting in the suppression of bipolar diffusion effect. In spite of the suppression of bipolar diffusion effect by K-doping, the power factor in K-doped compound is decreased significantly than the one of non-doped Pb0.5Sn0.5Te0.95Se0.05 compound. It indicates that when we increase chemical potential further on the breaking of topological band inversion, the thermoelectric performance is deteriorated because the chemical potential resides far from the linear band dispersions which become conventional material. The ZT for the K-doped (Pb0.5Sn0.5)(1-x)KxTe0.95Se0.05 is obtained as 0.91 at 750K for x=0.017 which is increased as much as 99% comparing to the pristine compound Pb0.5Sn0.5Te but it is reduced value (51.5%) comparing to those of Pb0.5Sn0.5Te0.95Se0.05 compound. We believe that this research is valuable on the confirmation that the weak perturbation of topological state and appropriate chemical potential tuning are important criteria in high thermoelectric performance [GRAPHICS]