4.6 Article

Compatibility of a Silicone Impression/Adhesive System to FDM-Printed Tray Materials-A Laboratory Peel-off Study

期刊

MATERIALS
卷 11, 期 10, 页码 -

出版社

MDPI
DOI: 10.3390/ma11101905

关键词

additive manufacturing; FDM; custom tray; peel-off strength; surface topography

资金

  1. China Scholarship Council (CSC) [201606240087]

向作者/读者索取更多资源

Computer-aided design (CAD) and additive manufacturing (AM) have shown promise in facilitating the fabrication of custom trays. Due to the clinical requirements, custom tray materials should achieve good bonding to the impression/adhesive systems. This study evaluated the retention of three fused deposition modeling (FDM) custom tray materials to a silicone impression/adhesive system before and after gritblasting (GB) by peel-off test. CAD-designed experimental test blocks were printed by FDM using acrylonitrile butadiene styrene (ABS), polyethylene terephthalate glycol copolyester (PETG), and high impact polystyrene (HIPS), and the reference test blocks were made of a conventional light-curing resin (n = 11). Before and after GB, the surface topography of all tray materials was analysed, and the maximum strength of the test block peeled off from a silicone impression/adhesive system was measured. After GB, the arithmetic mean height (Sa) and the valley fluid retention index (Svi) of the four material groups declined (p < 0.05). The peel-off strength of each of the four material groups significantly decreased by GB (p < 0.05), but no statistical difference could be found among them before or after GB. In all peel-off tests, adhesive failure occurred at the adhesive-impression material interface. The results indicated ABS, HIPS, and PETG could provide sufficient adhesion to the adhesive as the conventional light-curing resin, and GB could reduce the roughness generated by FDM and weaken the bonding between the adhesive and the silicone impression.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据