Coal tar pitch with a softening point (SP) of 78 degrees C is mixed with divinylbenzene (DVB) and then spheroidized by suspension method in dimethyl silicone oil for 1 h. During the spheroidization process, the mixtures of pitch and DVB are copolymerized due to vinyl in DVB. After vacuum-assisted heat treatment, the copolymer spheres can be stabilized completely and then carbonized directly at high temperature under Ar atmosphere without melting and deformation. After activation using steam at 850 degrees C for 1.5 h, spherical activated carbon (SAC) with smooth surface and specific surface area S-BET = 520 m(2 )g(-1) can be prepared. Further studies show that mesopore volume of the SAC is 0.29 cm(3) g(-1) , which accounts for 72.5% of the total pore volume. The good spherical morphology, smooth surface and rich pores (micropores and mesopores) can be attributed to appropriate copolymerization and vacuum-assisted treatment.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据