4.7 Article

Particulate migration behavior and its mechanism during selective laser melting of TiC reinforced Al matrix nanocomposites

期刊

MATERIALS & DESIGN
卷 82, 期 -, 页码 46-55

出版社

ELSEVIER SCI LTD
DOI: 10.1016/j.matdes.2015.05.041

关键词

Laser treatment; Metal matrix composites; Multiphase; Computational thermodynamics; Selective laser melting

资金

  1. National Natural Science Foundation of China [51322509]
  2. Outstanding Youth Foundation of Jiangsu Province of China [BK20130035]
  3. Program for New Century Excellent Talents in University [NCET-13-0854]
  4. Program for Distinguished Talents of Six Domains in Jiangsu Province of China [2013-XCL-028]
  5. Science and Technology Support Program (The Industrial Part), Jiangsu Provincial Department of Science and Technology of China [BE2014009-2, BE2014009-1]
  6. Fundamental Research Funds for the Central Universities [NE2013103, NP2015206]

向作者/读者索取更多资源

A transient three-dimensional model for describing fluid flow characteristics and particles migration behavior within the melt pool during selective laser melting (SLM) of TiC/AlSi10Mg nanocomposites was developed. The powder-solid transition, variation of thermophysical properties, and surface tension were considered in the model. The influence of laser energy per unit length (LEPUL) on heat and mass transfer, melt pool dynamics, and particles rearrangement was investigated. It showed that the Marangoni convection became more vigorous with an increase of LEPUL, accordingly enhancing the thermal capillary force. The high laser energy input induced a sufficient liquid formation and an improved wettability, lowering the friction force exerting on TiC solids. Under this condition, the reinforcing particles can be well mixed within the matrix. The experimental study on the distribution state of TiC reinforcement in the SLM-processed Al matrix was performed. The results validated that the dispersion of TiC reinforcement changed from a severe aggregation to a uniform dispersion in the matrix with the increase of LEPUL. The TiC reinforcement experienced a microstructural variation from the standard nanoscale structure with a mean particle size of 70-90 nm to the relatively coarsened submicron morphology with an average particle size of 134 nm as LEPUL increased. (C) 2015 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据