4.0 Article

The effect of a desensitizer and CO2 laser irradiation on bond performance between eroded dentin and resin composite

期刊

JOURNAL OF ADVANCED PROSTHODONTICS
卷 6, 期 3, 页码 165-170

出版社

KOREAN ACAD PROSTHODONTICS
DOI: 10.4047/jap.2014.6.3.165

关键词

Tooth erosion; Adhesives; Tensile strength; Lasers; Gluma dentin desensitizer

向作者/读者索取更多资源

PURPOSE. This study was aimed to evaluate effect of the desensitizing pretreatments on the micro-tensile bond strengths (mu TBS) to eroded dentin and sound dentin. MATERIALS AND METHODS. Forty-two extracted molars were prepared to form a flat dentin surface, and then they were divided into two groups. Group I was stored in distilled water while group II was subjected to a pH cycling. Each group was then subdivided into three subgroups according to desensitizing pretreatment used: a) pretreatment with desensitizer (Gluma); b) pretreatment with CO2 Laser (Ultra Dream Pluse); c) without any pretreatment. All prepared surfaces were bonded with Single Bond 2 and built up with resin composite (Filtek Z250). The micro-tensile bond test was performed. Fracture modes were evaluated by stereomicroscopy. Pretreated surfaces and bonded interfaces were characterized by scanning electron microscope (SEM). The data obtained was analyzed by two-way ANOVA (alpha=0.05). RESULTS. For both sound and eroded dentin, samples treated with desensitizer showed the greatest mu TBS, followed by samples without any treatment. And samples treated with CO2 laser showed the lowest mu TBS. SEM study indicated that teeth with eroded dentin appeared prone to debonding, as demonstrated by existence of large gaps between adhesive layers and dentin. CONCLUSION. Pretreatment with Gluma increased the mu TBS of Single Bond 2 for eroded and sound teeth. CO2 laser irradiation weakened bond performance for sound teeth but had no effect on eroded teeth.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.0
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据