Intrinsic Origins of Crack Generation in Ni-rich LiNi0.8Co0.1Mn0.1O2 Layered Oxide Cathode Material

期刊

SCIENTIFIC REPORTS
卷 7, 期 -, 页码 -

出版社

NATURE RESEARCH
DOI: 10.1038/srep39669

关键词

-

资金

  1. National Research Foundation of Korea (NRF) - Korean government (MEST) [2012R1A3A2048841]
  2. New & Renewable Energy Core Technology Program - Ministry of Trade, Industry & Energy (MOTIE), Republic of Korea [20152020105420]
  3. iBAT platform of the Industrial Strategic Technology Development Program - MOTIE, Republic of Korea [10041589]
  4. R&D Programs of National Research Council of Science Technology [CAP-14-2-KITECH]
  5. Korea Evaluation Institute of Industrial Technology (KEIT) [10041589, 20152020105420] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)
  6. National Research Council of Science & Technology (NST), Republic of Korea [CAP-14-02-KITECH] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)
  7. National Research Foundation of Korea [2012R1A3A2048841] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)

向作者/读者索取更多资源

Ni-rich LiNi0.8Co0.1Mn0.1O2 layered oxide cathodes have been highlighted for large-scale energy applications due to their high energy density. Although its specific capacity is enhanced at higher voltages as Ni ratio increases, its structural degradation due to phase transformations and lattice distortions during cycling becomes severe. For these reasons, we focused on the origins of crack generation from phase transformations and structural distortions in Ni-rich LiNi0.8Co0.1Mn0.1O2 using multiscale approaches, from first-principles to meso-scale phase-field model. Atomic-scale structure analysis demonstrated that opposite changes in the lattice parameters are observed until the inverse Li content x = 0.75; then, structure collapses due to complete extraction of Li from between transition metal layers. Combined-phase investigations represent the highest phase barrier and steepest chemical potential after x = 0.75, leading to phase transformations to highly Li-deficient phases with an inactive character. Abrupt phase transformations with heterogeneous structural collapse after x = 0.81 (similar to 220 mAh g(-1)) were identified in the nanodomain. Further, meso-scale strain distributions show around 5% of anisotropic contraction with lower critical energy release rates, which cause not only micro-crack generations of secondary particles on the interfaces between the contracted primary particles, but also mechanical instability of primary particles from heterogeneous strain changes.