Recovery of lithium and cobalt from waste lithium ion batteries of mobile phone

期刊

WASTE MANAGEMENT
卷 33, 期 9, 页码 1890-1897

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.wasman.2013.05.008

关键词

Leaching; Cobalt; Lithium; Recycling

资金

  1. Department of Science & Technology, Government of India

向作者/读者索取更多资源

In view of the stringent environmental regulations, availability of limited natural resources and ever increasing need of alternative energy critical elements, an environmental eco-friendly leaching process is reported for the recovery of lithium and cobalt from the cathode active materials of spent lithium-ion batteries of mobile phones. The experiments were carried out to optimize the process parameters for the recovery of lithium and cobalt by varying the concentration of leachant, pulp density, reductant volume and temperature. Leaching with 2 M sulfuric acid with the addition of 5% H2O2 (v/v) at a pulp density of 100 g/L and 75 degrees C resulted in the recovery of 99.1% lithium and 70.0% cobalt in 60 min. H2O2 in sulfuric acid solution acts as an effective reducing agent, which enhance the percentage leaching of metals. Leaching kinetics of lithium in sulfuric acid fitted well to the chemical controlled reaction model i.e. 1 - (1 - X)(1/3) = k(c)t. Leaching kinetics of cobalt fitted well to the model 'ash diffusion control dense constant sizes spherical particles' i.e. 1 - 3(1 - X)(2/3) + 2(1 - X) = k(c)t. Metals could subsequently be separated selectively from the leach liquor by solvent extraction process to produce their salts by crystallization process from the purified solution. (C) 2013 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据