The cavitation resistance of a stainless steel and two flame thermal spray coatings was tested in laboratory according to ASTM G32 standard. The time-variation curves of cumulative volume loss, erosion rate and roughness parameters were related to the microstructure of the samples and to the wear mechanisms. Pores, unmelted particles and other microstructure defects prevented the coatings from showing an incubation period during the tests, while the stainless steel exhibited the expected incubation, acceleration and maximum rate stages. In the stainless steel, a correlation between the transition from incubation to acceleration stage and the R-sm/R-q and R-y/R-q ratios was established. (C) 2010 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据