Effect of Iron Slag on the Corrosion Resistance of Soda Lime Silicate Glass

期刊

SILICON
卷 10, 期 1, 页码 11-20

出版社

SPRINGER
DOI: 10.1007/s12633-015-9340-5

关键词

Silicate glass; Iron slag; Glass durability; SEM

向作者/读者索取更多资源

Soda lime silicate glasses containing different amounts of iron slag 0-30 % were prepared. The chemical durability of the prepared glasses was examined by immersion in HCl or HNO3 solutions at room temperature. The results show that the glass durability increases with increasing the amount of slag in the glass composition to a certain amount, then followed by a decrease in the glass durability. Various mechanisms of corrosion and the role of the mobility of cations and their leaching into solution, also the effect of time of leaching are discussed. The densities of all glass compositions were measured. The quantitative analysis obtained from infrared absorption spectra in the range of (400-4000) cm(-1) in relation to the effect of corrosion on the absorption spectra has been studied in terms of structural concepts. The topography of the glass surfaces was observed by scanning electron microscopy (SEM). The concentration percentage of the ions present on the glass surface was determined by Energy Dispersive X-ray analysis (EDX).

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.3
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据