4.4 Article Proceedings Paper

Temperature dependence of Fluorine-doped tin oxide films produced by ultrasonic spray pyrolysis

期刊

THIN SOLID FILMS
卷 518, 期 4, 页码 1241-1244

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/j.tsf.2009.05.064

关键词

Fluorine doping; Fluorine concentration; Tin oxide; Spray pyrolysis; SIMS

向作者/读者索取更多资源

Fluorine-doped tin oxide (FTO) films were prepared at different substrate temperatures by ultrasonic spray pyrolysis technique on glass substrates. Among F-doped tin oxide films, the lowest resistivitiy was found to be 6.2 x 10(-4) Omega-cm for a doping percentage of 50 mol% of fluorine in 0.5 M solution, deposited at 400 degrees C. Hall coefficient analyses and secondary ion mass spectrometry (SIMS) measured the electron carrier concentration that varies from 3.52 x 10(20) cm(-3) to 6.21 x 10(20) cm(-3) with increasing fluorine content from 4.6 x 10(20) cm(-3) to 7.2 x 10(20) cm(-3) in FTO films deposited on various temperatures. Deposition temperature on FTO films has been optimized for achieving a minimum resistivity and maximum optical transmittance. (C) 2009 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.4
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据